As a user, you should be familiar with the correct operating procedures for short cycle laminating hot press. It should be noted that only by maintaining normal and reasonable operations can its performance be fully utilized, and at the same time it can also improve product quality. So what are the specific operations? Next, we will briefly introduce the operation method of the short cycle veneer hot press and hope to be helpful.

 

First of all, it should be noted that before starting the short cycle laminating hot press, a series of inspections should be carried out. The main task is to check whether the screws and fasteners are well-fastened and loosened. If any, tighten the fasteners in time. At the same time, we must also pay attention to checking whether the oil level in the accumulator and the fuel tank is normal and whether the oil quantity is sufficient, and add it in time. Also pay attention to ensure the quality of the entire machine lubrication.

 

Of course, in the actual operation of the short cycle laminating hot press, the final quality is closely related to its temperature. Therefore, it is also necessary to check whether the temperature of the equipment can meet the specified requirements, and check whether there is leakage or the like. Note that before operation, you should check the workbench surface for debris, dust, etc. If necessary, clean it in time.

 

After inspection, a short cycle veneer hot press should be started to bring it into working condition. During the operation of the equipment, the staff should pay attention to see if the piston is moving smoothly, with no jitter or crawling. When the hot press reaches the maximum working pressure, there is no oil leakage in the seal ring. At the same time, we must also pay attention to check the operation of the oil pump and whether the temperature rise is normal, and whether the temperature of the oil is normal. Motor load, temperature rise, etc. also need to be inspected to ensure that switches and actions are sensitive and reliable.

 

In addition to these, it is also necessary to inspect the heat-conducting oil hose joints of the short cycle laminating hot presses for oil leakage, etc., and whether the valves are operating normally. In short, we need to conscientiously study and master the operation skills of the short-cycle veneer hot press to understand its operation in a more comprehensive and reasonable manner.

 